Jingliu refers to straight or irregular straight strips on the cloth surface along the warp direction, which appear as refractive differences on the woven fabric. Jingliu is one of the most common and most difficult to cure defects in water jet weaving mills, which has a great negative impact on the product quality and economic benefits of enterprises. So how to overcome this defect is always one of the topics explored in the field of production technology of weaving enterprises.


The main reasons for Jingyan production


1.Filament factors


The influence of the raw silk is very complicated, mainly including uneven thickness, different cross-sectional shapes, different single fiber numbers, and different TiO2 content. During the spinning process, the differences in the actual process technology control between each spindle, the environmental temperature and humidity, and the processing time period will cause differences in fiber crystallinity and polymerization.


2. Weaving processing factors


There are also many factors that induce warp willows in various processes of the weaving factory, but they can be summarized into three aspects: First, the difference in tension. The difference in tension causes the elongation of the threads to be different, which makes the refractive index different. The other is that the surface of the silk thread is damaged, which causes uneven reflection of the silk thread or the surface of the silk thread is damaged, which causes the difference in dyeing performance. The third is environmental factors. The different environmental conditions including temperature, humidity, and light make the physical properties of the yarn different, and the degree of deformation under the same tension causes the difference in refractive index.


3. Post-dyeing processing factors


There are two main points: First, the desizing is not clean, which causes the slurry to be colored. The second is the improper leveling control resulting in uneven color absorption between the threads.



Measures to be taken to resolve Jingliu


1. Raw silk


Strengthen the physical property inspection of the raw silk to determine whether to feed or use it accordingly. Strictly dye the sample on the cloth head and adjust in time if problems are found. If time permits, the upper row of wires can wait for the small axis sample before deciding whether to continue warping.


2.Weaving


For weaving production, prevention must be the main focus, we cannot wait for problems to occur, and then look back for the cause. First of all, it is necessary to strengthen the batch number management of the raw silk and the balance management of the upper row. It is necessary to ensure an equilibration time of more than 24 hours before the start of warping, so that the original silk stored under the condition of large differences in ambient temperature and humidity will be moisture-balanced. The upper wire also requires the production date interval to be as short as possible, and the size on the tube must be uniform. The tension of each process is controlled uniformly. And complete the configuration and clean control of the silk channel, such as the creel tensioner, telescopic joint seams, each channel teeth, each roller and other guide wire components should be smooth and clean. In short, no factors that cause uneven tension are allowed. Third, we must strengthen the management of temperature and humidity, especially the temperature and humidity of the warping creel, the shaft and the weaving site, should be equipped with a suitable air conditioning system (including ventilation, humidity Wait). The density of the healds should be reduced as much as possible. The setting of the process parameters of the loom should ensure that the water jet cannot hit the warp. The slurry should choose a slurry with stable performance, good film formation, strong adhesion but low viscosity, and when the summer comes, the manufacturer should be asked to increase the Tg value of the slurry film to more than 20 ° C.